Model: SLHG-1
Suitable process and application: Shielded atmosphere furnace welding, aluminum-aluminum alloy, copper-aluminum,suitable for welding in situations where low soldering temperatures are required
Appearance and specification: light gray paste
Brazing temperature: 520-560℃
Brazing temperature: 520-560℃
Applicable process: Shielded atmosphere furnace welding, aluminum-aluminum alloy, copper-aluminum,suitable for welding in situations where low soldering temperatures are required
suitable for welding in situations where low soldering temperatures are required.