Product detailsParametersProcessApplication
Model: BAg72Cu
Suitable process and application:Shielded atmosphere furnace welding, can weld copper, steel and other materials.
Composition: Ag:24~26;Cu:40~42;Zn:Bal
Appearance and specification: Gold, - 160 mesh
Melting point (melting range): 700-790℃
Melting point (melting range):700-790℃
Applicable process: Shielded atmosphere furnace welding, can weld copper, steel and other materials.
Powdered silver-copper solder is usually used to connect copper or copper alloys, and also can be used for brazing stainless steel, carbon steel, and nickel-based alloys. It has good conductivity and thermal conductivity, and is widely used in vacuum devices and electronic components.